3-yr aniv. sale no bargain,0.2mm nozzle clogged after 2 yrs clog-free

Have you always used the same filament type or have you changed from I don’t know, PETG to ABS to PLA? If that’s the case, I found with my limited experience with 0.2 nozzles that purging temperature might not be high enough, purge longer at higher temperature to make sure the nozzle is clear from previous higher temp filament. 0.2 nozzles can be tricky.