Thanks for you thoughts… the desiccant I’m using is 10% Orange beads that turn dark when the desiccant is becoming saturated. The desiccant pictured is fresh. I didn’t dry the PETG though (noob). I just took it out of it sealed bag and put it in the AMS a week ago when I set up the system. In another post I’ve indicated that the AMS Hydrometer seems to be reveling positive signs as to the Humidity level in the AMS. Also the first print I made with this material turned out well.
Oh and my Bambu Basic PETG settings are as follows…
Filament:
Cooling: