It’s been a minute, but wanted to give a final follow up. Even though changing the initial flow ratio seemed to help with PLA adhesion, I still had issues with the first layer having the “cat’s tongue” texture described by OP, and I continued to have extremely poor success with PETG. The following picture shows the kind of results I got with PETG using default settings:
This next picture is as good as I could get it when tweaking the initial flow ratio and selecting “Textured PEI Plate” in BambuStudio (basically just to raise the bed temperature to 80C) – but keeping the SuperTack on the printer. Even though it was somewhat passable, the adhesion of the PETG was still not great and could be peeled off easily, even while the bed was still hot.
After continual print failures (even with PLA), I found this article which has instructions to tighten the 4 screws on the back of the hotend heating assembly.
When I checked, all 4 screws were loose on my A1
. After tightening the screws, my first layers were noticeably better, but still far from perfect. Long story short, I ordered a new hotend heating assembly. The first test print with PETG after installing the new hotend turned out beautifully when using default settings.
And for reasons I don’t understand, the layer adhesion was surprisingly strong – a complete 180 from before replacing the heating assembly – and I struggled to get the test print peeled off the plate.
So, at least in my case, it seems as though I needed a new hotend heating assembly.