Elegoo PLA+ stringing on P2S

I’m trying to solve Elegoo PLA Plus (Black) filament stringing on P2S printer.
I tried all the suggestions I found in another threads “improve” stringing with no change at all (temp/flow/retraction calibration, filament drying).

My Filament profile is configured as a “copy and paste for each and every value” for PLA+ profile in Elegoo slicer.
My Room-temp is about 25 degree celsius (I saw posts where peope suggests that same issue happens in low-temp conditions).
I dried filament several times, and the last test was done after drying it down to 8% humidity (reported by AMS2), while there is still no difference at all from the initial test results I had.

Any suggestion how to resolve this?

Hello, the same for me and when I do Hueforge, it’s not very clean and even ugly compared to A1 that is perfect. Some says the temperature of the P2S case is a factor, some says retraction could influence but I didn’t test. I use to use a lighter to remove theses stringings. It’s not very practical for hueforge cause it can warp the plastic regarding the widthness.

I’m having the same problems with this filament on my A1. Reduced the nozzle temperature from 220°C to 190°C but the problem still persists.

Maybe this filament just isn’t that great. I think I’ll buy eSUN the next time and see if it’s better.