Esun PETG > Messy

I have no problem with eSUN PETG although my experience is it needs drying straight out of the bag.

Check like this Help troubleshooting PA6-CF issue - #25 by ZiggyP

After that your temperature is high my eSUN PETG says 250C max and I print at 235 (the higher the temperature the worse mess wet filament makes). PA also looks high I would expect around 0.035. Wet filament will mess up PA calibration.