Hey, does anyone have any ideas about the ripples on the first layer? I’ve already tried what’s in the wiki, but unfortunately without success. I’m using H2D, PLA BBL Basic, and the bed is clean. I’m having the same problem with the original plate as well. Best regards, Vakarian

Looks like an after-market plate. How does the stock Bambu plate print?

Have you ran all the calibrations? Did you check the box for high temp calibration?

This is the cryogrip frostbite that does not want to be set at high temp. I don’t think hi-temp calibation with an other plate will help low temp calibration of that particular plate.

I think cleaning agent used was not appropriate, I would start by cleaning it again with dish soap (no additives) and water and scrub with a soft brush.

1 Like

The nozzle is too close to the bed in some spots, but not others. Like the bed continued to change shape after bed leveling. I was just thinking of what would affect the leveling or offset.

He says he had the same problem with the original plate. So I was looking for something non plate related.

Looks like its sticking well, but too close and the leveling is off

The bed adhesion is good; I cleaned the plate exactly the same way I clean the plates on the X1C (where this problem doesn’t occur).

I’ve already performed all calibrations, including the high-temperature calibration, multiple times. I’m using the latest firmware and the latest version of Bambu Studio.