Hello everyone, after printing 1kg of PETG HF on the Bamboo H2D with the second nozzle, the pieces start to come out like this.
What do you think it could be?
Hello everyone, after printing 1kg of PETG HF on the Bamboo H2D with the second nozzle, the pieces start to come out like this.
What do you think it could be?
How are you drying your filament? Looks like a moisture issue to me.
It was not dry. It was opened and started printing immediately. Whoever works with the machine does not want to dry the filament.
Can it be dried inside the machine?
Anyway
It can be dried in the AMS 2 Pro or AMS HT if you have one connected. There is also a procedure for drying inside the build chamber but I don’t think it works very well.
It’s not safe to assume that filament is dry from the packaging.
Use the heatbed …
Or AMS2 Pro, or AMS HT, or an Oven, or a Food Dehydrator, or an AirFryer, …
Sometimes I am very jealous of the people who just buy an H2D and don’t even consider drying… Almost like buying a yacht and park it in the dock paying the maintainance fees and dock rents for years without realizing that the boat can sail.
Thanks, I’ll try to dry it inside the machine.