PETG HF w/ .6 Tungsten Nozzle on H2D cannot be tuned to satisfaction

I’ve been struggling for 3-4 days printing with this filament. I’m seeing stringing and zits. I’ve dried the filament twice in the HT AMS and that has not helped.

I’ve tried the dynamic flow and flow rate calibrations with very little improvement in results.

if you’ve used this combination, what settings have worked for you?

Is it possible that I’m just printing a model that’s not going to cooperate with this material? I’m not printing anything highly detailed.

Which color, and are you able to tune it with a normal .4 nozzle?

Black, and I’ve had better results with the .4, but I’ve still never quite gotten it right.

Maybe a dumb question but needs to be asked. Do you have the printer set for a .6 HF and in the slicer?

Yes, the printer screen shows that it recognizes the nozzle as a .6 TC HF nozzle. The filament settings in slicer are set for .6 HF. I’m not sure if theres a software option to set the nozzle material to TC in the slicer or not. It may even be there already somewhere.

If the nozzle under the printer setting is set for the HF then you are good. The printer will alert you if the sliced nozzle is different than the one you’ve set on the printer screen.

Was just a thought.

Ah yes, it is set to 0.6/HF under printer.

1 Like