Trying to improve the finish on flat/top surfaces when printing TPU85. Any suggestions on how to improve the print quailty. I have printed 5 of these and 2 have had these imperfections. The last photo is the best print.
dry your filament.
increase the infill ratio.
feed from TPU inlet using the assist motor and a dry box.
I have it in a HT AMS and using the feed assist module. Is the small pitting from it having moisture?
yes, it’s from moisture.
dry it again and print the desiccant holders to keep it dry ![]()
Any other suggestions. Is this an over extrusion?
I recommend that you turn down the movement speed! It worked for me, but if it does not work for you, let me know and I will do what I can.