Cross-post here. AMS 2 Pro RH reading can be misleading. Crosscheck independently with sensors that can read below 10%.
Direct Answer: if you print PETGs, hydroscopic PLA variants (CF, Wood etc.), engineering materials, “8% on the AMS” is when the pods should ideally be changed as soon as possible. (probably a different value on units that reads RH correctly)
(If you refilled it jam packed fresh but the readings aren’t go down back to “0% on the AMS” (5%~8% real RH) within ~half a day, it’s sign that some rolls are wet and are releasing moistures)