H3C: Frayed outer edges only with manual K value, clean with auto Flow Dynamics

Hi all,

I’m tuning a custom PETG profile (JAYO PETG HS Matte, created via “Create Custom Filament”, based on Generic PETG) on my H3C, 0.4 mm standard nozzle. All test cubes were printed on the same tool head, nozzle 250 °C, bed 70 °C, retraction 0.8 mm, extra length on restart off.

  • Flow Dynamics Calibration = On (auto): clean outer edges, but some blobs on bridges/overhangs and a slight indented band where overhangs start (cube 4).
  • Manual K (0.02, 0.03 and 0.04, calibration unchecked at print start): cleaner overhangs, less stringing, but frayed/ragged outer edges at the cube corners, always at the same heights (where the window openings begin/end, cubes 5 and 6).

The fraying looks identical at 0.02, 0.03 and 0.04, so it doesn’t seem to depend on the K value itself. A PA line test shows 0.03 as best.

Does the auto calibration on the H3C do more than just set a single K value (e.g. speed-dependent compensation)? Has anyone seen similar behaviour with manual K values on H2C/H2D/H3C?

Photos attached. Thanks!