I am trying to print a “card” like surface in the sense that its thin , i am using a 0.2mm nozzle on my bambu a1 mini with atextured plate , yet its constantly ripping a hole in the beggining of the print .
Also what i have noticed is that while its printing the surface is kinda ruff , with little “hairs” sticking out.
The most probably cause of this issue is contaminantes like finger oils on your build plate causing adhesion issues. Clean your build plate with dish soap (Dawn) and hot water. Give it a really good scrub and be sure not to touch the build plate afterwards.