Hello all, I’ve hit a wall on trying to figure out why my infills have been choppy and not complete. The walls seem to print fine it’s just the infills that have issues.
It may be due to moisture, but I don’t know for sure. Ambient humidity near the AMS is 50%.
Any help is appreciated!
Infill is printed faster than walls so the printing temperature may not be high enough. That being said I would suggest using a non crossing infill such as Gyroid and I would suspect this will solve your issue.
2 Likes
Thanks for the response. My last piece was gyroid infill and it was much much worse. I even upped the nozzle temp for the yellow PETG and it still looked bad but the gaps with rectilinear were smaller so I just went with that.
If you print in “Silent” mode does the infill print better?
I will find out in about 12 hours 
Thanks.