P1S and Orca Slicer
PolyLite ASA
Temp: 260c
Bed: Textured PEI at 100c
Flow Rate: 0.9405 (previous was 0.95)
Pressure Advance: 0.018 (previous was 0.02)
4 top layers, 0.2 nozzle, 10% gyroid
I’m trying to tune this filament because the default profile isn’t giving me a good top layer, it’s very rough. This is after tuning flow rate and PA. I’m wondering if I picked the wrong number on the flow rate or PA