Hello everybody. I’m a beginner, the first time I write on the forum. I have a 1p1 for 3-4 months, I haven’t used it for 1-2 weeks and lines started to appear on the outer walls at different heights as you can see in the pictures. If anyone has encountered this problem before or guess what it might be, please give me some advice. Thank you
Basic bambu Pla
Temp 210-220