I see that you have not enabled Pressure advance , are you still using automatic will not work on PEI, and not sure if it is done first on other plate is it really going to remember it
Calibrate PA - tower method
my PA for ASA is 0.047 , but what i found is that 0.05 works almost for any ASA and ABS i have , but still fine tune it with tower method
-Plate temp is at 100C , i had some times issues with 100 that is why i use 110C, the actual temp is lower what you set by a few degrees anyway
Make sure that you increase Temp of vitrification to 110C as if you have the script will will cause to turn on the chamber fan
Speeds are well too fast for ASA and for me was causing warping when i started with ASA - either reduce the volumetric speed from 18mm3/S down to 10mm3/S for a test , or change all the speeds down to 140mm/S ( outer wall , inner wall, infills etc )
But I will try on my bambu black PEI ( not the gold one ) next few days and let you know as i still have prints and use engineering plate at the moment .
Edit: all my suggestions were assuming that there is no real problem with bed adhesion with PEI, but if it is, here is a good thread , i like most the sandpaper 400 or 1000 Grid idea from @mikeoxlong420 and from @Rom3oDelta7