Overhangs on honeycomb pattern

Anything I can do to make these overhangs better and also improve those weird horizontal line bulges?

  • Elegoo PLA+, 205 nozzle temperature, 60 bed temperature
  • Between 10mm/s and 25mm/s on these overhangs, confirmed in the slicer. 40mm/s outer walls and 55 inner walls for the rest, 30mm/s external bridges
  • 100% cooling for overhangs greater than 25%
  • Inner/Outer wall order.
  • Flow ratio of 0.985 and k value at 0.035 after calibration.
  • Minimum layer time at 16s.
  • Ran at a 0.12mm layer height on a 0.4mm nozzle.

I do notice some speed changes around this area… Are things overly slowed down or something?

205* is too cold for PLA+, it should be more in the 215* - 220* range.