PETG-HF is a DISASTER imho

Generally good but the first photo has a bit of a doughy-looking surface which is how just a bit too much water in the filament manifests on my printer.

With dried filament I see very smooth surfaces with much reduced effects that highlight the layer lines. I thought I had posted photos in this thread but know I have in other PETG HF problem threads. The difference between wet and dry is very noticeable and doughy-looking surfaces seem to be a sign of water content being a little too high.

Here they are: New X1E - PETG HF problems - #3 by MZip