Wondering if could get a little help? Have been using my P1S for about a mount printing odds and ends making no changes in Bambu studios.
Recently printed an EGO battery holder and decided to make a few changes, the result not so great.
Using Bambu PLA I decided to clone holder to 4 and increase speed to sport as well as increasing hot end from 200 to 220.
The first 2/3 of holder were excellent then on the top 1/3 on all 4 it became textured and showed all the uneven layer lines.
Currently trying a single without the changes. Any ideas as to what may have gone wrong?
2 Likes
Check the nozzle for clogs and check the silicone sock. It might also be an issue with the extruder gear.