Pla filament Enotepad - wood, I used a generic profile, changing only the temperature (lowering it) what could these defects depend on?
Help me
Thats easy, you are printing way too fast with a generic profile… Your first layer looks fine because it gets printed at 40mm/s. Maybe you could push it to 50-80mm/s when printing, but i would not go any faster.
1 Like
I find that using the Silk PLA profile suits wood filament better, as it prints slower.
2 Likes
you can limit the “max volumetric speed” for this filament.
According to this calculator: Volumetric Flow Rate Calculator for 3D Printer - YogiTech
This would leave your profile untouched, but will slow down the print speed for this specific filament
3 Likes
Thanks to your advice, I fixed it