Rough wall finish on Fine profile

Having some issues with the surface quality on a print when using the Fine (0.12) profile using a generic PLA profile.
It looks like underextrusion on longer stretches of flat surfaces because it’s broken up by sharper curved details. Is this correct or can someone identify the cause?

1 Like

I have the exact same issue.
Tried changing it to print outer walls first, no luck.
Only showed up on one side

Did you ever figure it out? I’m having the same issue.

I am also having same issue. any solution?
IMG_2404|666x500

It was solved by cleaning extruder gears.