I’m struggling with these gaps in the first layers. I’m using Bambulab Matte PLA, Settings: Arachne wall generator, hot plate, 0,16 mm High Quality profile, tried to slow down speed to 25 mm/sec for first layer and 50 mm/sec for first layer infill and tried to increase flow rate to 1.08. Any suggestions?
The filament lines should not be that prominent anywhere on the bottom surface.
Don’t just pick a flow number out of the air. Calibrate the filament and the default speeds will work well.