I myself use a Sunku S2 and an older Enisia. Nothing special, but good for PLA, PETG and TPU while higher temp filaments take longer or go on my build plate for drying. There are quite a few good discussions on driers in the forum. What is the 3d filament dryer you choose?.

When drying, make sure not to exceed the recommended temps for the filament though as that could bind the strands. That can make the filament unusable. So do not use 90-100°C for PLA, PLA-CF.

Also note that the recommended build plate temps are not the actual chamber temps. That tends to be quite a bit lower.